Skip to content
Stainless Steel Repair Sleeve for Tee Fittings

Stainless Steel Repair Sleeve for Tee Fittings

This is the tee version of the all-stainless split sleeve: a formed shell covering the run, the branch and the junction, in the same alloy family as the pipe. A hygienic or corrosive line cannot take a junction…

Also known as: Stainless Steel Split Repair Tee, Stainless Steel Tee Repair Clamp

BS-RCTE-SS
Size Range DN15–DN4000
Sealing Pressure ≥1.6MPa (232 PSI)
Body Material SS304 / SS316L / Duplex 2205
Coating None (Stainless Steel Body)

Usually replies within 24 hours sales@baoshuopipe.com

Technical Specifications

Part Number BS-RCTE-SS
Size Range DN15–DN4000 · Stainless Steel DN15–DN4000 · Custom sizes available beyond the above range
Body Material SS304 / SS316L / Duplex 2205
Seal Material EPDM / NBR / FKM
Sealing Pressure ≥1.6MPa (232 PSI)
Bolt Specification M16×80, Grade 8.8 High-Strength Bolts
Coating None (Stainless Steel Body)
Length Range 200–600mm (7.9"–23.6")
Weight 1–1927 kg (approx)
Applicable Pipe Types Steel, Stainless Steel, Ductile Iron, PVC
Working Conditions Standard Pressure, Corrosion Resistant

Custom Orders Available

This product can be customized to your specifications. Contact us with your requirements.

Request Custom Quote

Check the fit before ordering.

Measure the actual pipe
Nominal DN alone does not define the outside diameter. Confirm the pipe material, measured OD and condition.
Confirm the geometry
Provide dimensions of the connection or damaged area. Product shape, sealing length and end connections must match the job.
Match the seal to the service
Confirm medium, temperature and pressure together. A material name alone is not a service approval.
Plan a safe installation
Pipe integrity, isolation and installation procedure require a site-specific assessment. Suitability for live service must be confirmed.
Read the full technical guide7 chapters · complete product description

Product Overview

This is the tee version of the all-stainless split sleeve: a formed shell covering the run, the branch and the junction, in the same alloy family as the pipe. A hygienic or corrosive line cannot take a junction part that introduces a different metal into the crevice, and a junction is the hardest place to weld a patch into without a purge.

Where it is used

  • Stainless process pipe with welded or mechanical branch junctions
  • Food, pharmaceutical and fine chemical plants
  • Branch connections where a welded patch would need a purge
  • Corrosive service where the junction is the leak point

Choosing the right build

Run and branch outside diameters, plus the length over the junction, are what the shell is formed from; both sizes are needed before it can be built. A four-way junction in the same material takes the stainless cross sleeve; both are listed on the stainless steel series page.

How a formed tee shell closes a junction

A junction has three sealing lines to close, not two: up the run on both sides of the branch, and around the branch collar itself. That is why the shell cannot be a tube with a hole in it. A formed tee shell is pressed so the run bore and the branch bore meet in a smooth compound curve, and the gasket is cut as one continuous piece that follows the run, turns up the collar and comes back down. If the gasket is made as three strips or two pieces, the ends meet in a butt joint right at the corner where the surface curvature is highest, and that corner is the first place to weep.

The bolt load has to be shared between the two directions. Bolts running across the run close the run bands; bolts across the branch close the collar. Tightening one direction before the other pulls the gasket away from the other pair of bands, so the sequence matters as much as the figure you tighten to.

Unlike a welded patch, the sleeve adds its section around the junction without putting more heat into metal that has already been welded at least twice.

Installation

  1. Identify the junction type first. A welded saddle, an extruded outlet and a threaded boss present very different external geometry, and the collar is formed around whichever you have.
  2. Clean the run and the whole branch collar to bare metal, including the weld fillet or the threaded boss root. Grit and old paint trapped under the collar hold the gasket off the surface.
  3. Measure the branch projection — the length of branch pipe standing proud of the run — and the run and branch outside diameters. Note the distance from the junction to the nearest fitting or weld on the run.
  4. Dry-fit the shell and check that both run bands and the full collar touch. Look for a gap where the collar meets the run; that gap is where the gasket will not be compressed.
  5. Fit with the gasket and set the shell so the collar is centred on the junction, not offset towards one side. Mark the run before closing.
  6. Tighten the run bolts first, in two passes alternating across the shell, then bring the branch bolts up to the working figure. Going the other way traps a fold of gasket in the collar corner.
  7. Re-check the run bolts after the branch bolts. Closing the collar moves the shell slightly, and the run bands loosen as it does.
  8. Pressure-test with the junction exposed. Watch the collar corner and the point where the collar meets the run — both leak sites appear there before anywhere else.

The frequent error is to tighten the branch bolts to full figure first because they are easier to reach. The collar then pinches, and no amount of work on the run bolts recovers the gasket once it has taken a set in the wrong position.

What we need to quote the junction

A tee shell is formed per junction, so these come before anything else:

  • Run outside diameter and branch outside diameter — both, separately
  • Branch projection, measured from the run surface to the end of the branch stub
  • Junction type: welded saddle, extruded outlet, or threaded boss
  • Run length available each side of the junction, so the shell does not foul the next weld or fitting

Then the service data: medium, normal and maximum temperature, line pressure, and whether the branch is insulated or lagged separately from the run. A branch that is lagged to a different thickness changes what room the collar has.

A photograph of the junction with a tape measure across the run and up the branch resolves more questions than any form. Because the shell is formed around the projection, a drawing returned for confirmation before forming is the most reliable way to avoid a part that does not fit. For a four-way junction the same information is needed on all four legs, and the part is the stainless split repair cross.

Where a tee sleeve is the wrong part

The part works on a junction that is sound apart from the leak. It does not work where the junction has moved.

  • A branch that has been pushed or pulled out of square. If the branch is no longer at right angles to the run, the collar cannot seat on both the branch and the run at once. Using two separate sleeves — one on the run, one on the branch — is not a substitute either, because neither closes the corner.
  • A crack running along the weld seam. A crack that propagates along the fillet will keep going under the shell. Fit a sleeve over it and you have covered a crack you can no longer see. Cut out and reweld, or use the weld seam repair clamp only where the seam defect is a pinhole and not a running crack.
  • Oval or deformed run. The run bands need a round surface. A run that has been squeezed or dented at the junction will bridge and leak.
  • Long circumferential wall loss on the run. A sleeve seals; it does not restore a run of pipe that is thin over a length. Where the wall loss runs longer than the shell, replace the spool.
  • A threaded branch that has to stay serviceable. If the branch must be opened or a fitting removed later, the collar over the boss takes that access away. A repair clamp with threaded outlet keeps an outlet available instead.

Alloy and gasket selection at a junction

The shell is supplied in SS304, SS316L or Duplex 2205 under ASTM A240 / GB/T 3280. At a junction the choice matters more than it does on a straight run, because a junction is a crevice by geometry: the collar makes a pocket between shell and pipe where the medium sits and concentrates. A shell in a different alloy from the pipe becomes the anode in that pocket.

  • SS304 where the pipe is 304 and chlorides are low.
  • SS316L for chloride-bearing process streams, coastal installations and washdown areas.
  • Duplex 2205 where chloride stress corrosion cracking is the risk and a higher-strength shell is wanted at the collar.

The gasket runs as a single continuous piece in EPDM to BS EN 681-1 / GB/T 21873, NBR to BS EN 681-2 / GB/T 21873, or FKM to ASTM D2000 / ISO 1629. EPDM is the default for potable and waste water but not for mineral oil; NBR suits hydrocarbon service but not ketones or ozone; FKM covers higher temperatures and a broader chemical range. The comparison is set out in EPDM, NBR, FKM and silicone compared.

Fasteners are SS304 to ASTM A193 / GB/T 3098.6, so the assembly adds no dissimilar metal. The design working pressure is 1.6 MPa and the size range is DN15–DN4000. AWWA C230 covers full-encirclement repair clamps for water service and is worth naming as the industry reference for this family of part; the grades are set out on the stainless steel series page.

Documents

Series Handbook Stainless Steel Series Browse the full series or download the handbook for complete specs.

Warning: Undefined array key "rcte-ss" in /www/wwwroot/baoshuopipe.com/wp-content/themes/astra-child/inc/helpers.php on line 1806

Also available in carbon steel: Repair Sleeve for Tee Fittings

Related Products

Corrosion-Resistant Repair Sleeve

DN15–DN4000

The interior fluoroplastic barrier protects its covered shell surfaces, while FKM provides the seal; confirm both for…

NBR-Sealed Repair Sleeve

DN15–DN4000

NBR-sealed repair clamp for petroleum, lubricant and fuel lines — hydrocarbon service that swells and destroys EPDM…

High-Temperature Repair Sleeve

DN15–DN4000

The supplied silicone VMQ seal requires confirmation for the actual fluid, phase, temperature, pressure and thermal…

Need a different spec?

We customize size, material, seal, and coating to your requirements.

Request Custom Quote
Scroll to Top